OPTICAL FIBERS WITH LOW BEND LOSS

发明专利审中
9浏览
20权利要求 · 1 独立
§ Ⅰ

卷宗概要

发明人

Snigdharaj Kumar Mishra; Pushkar Tandon

IPC 分类

G2B 6/2G2B 6/28G2B 6/36

CPC 分类

G2B6/2071G2B6/2104G2B6/281G2B6/3638

An optical fiber may include a core region and a cladding region surrounding the core region. The cladding region may include an inner cladding region surrounding the core region, a depressed-index cladding region surrounding the inner cladding region, and an outer cladding region surrounding the depressed-index cladding region. The inner cladding region may include a thickness greater than or equal to 1 μm. The depressed-index cladding region may include a first region and a second region, wherein a relative refractive index of the depressed-index cladding region may decrease monotonically with increasing radius in the first region, and wherein the relative refractive index of the depressed-index cladding region may be substantially constant in the second region. The optical fiber may achieve low microbend loss with large mode field diameter, while also maintaining low macrobend loss, low cable cutoff, and/or a zero dispersion wavelength between 1300 nm and 1324 nm.

原文(中文)

An optical fiber may include a core region and a cladding region surrounding the core region. The cladding region may include an inner cladding region surrounding the core region, a depressed-index cladding region surrounding the inner cladding region, and an outer cladding region surrounding the depressed-index cladding region. The inner cladding region may include a thickness greater than or equal to 1 μm. The depressed-index cladding region may include a first region and a second region, wherein a relative refractive index of the depressed-index cladding region may decrease monotonically with increasing radius in the first region, and wherein the relative refractive index of the depressed-index cladding region may be substantially constant in the second region. The optical fiber may achieve low microbend loss with large mode field diameter, while also maintaining low macrobend loss, low cable cutoff, and/or a zero dispersion wavelength between 1300 nm and 1324 nm.