検索に戻る
案件記録

CERAMIC SUBSTRATE, CERAMIC CIRCUIT BOARD, SEMICONDUCTOR DEVICE, METHOD FOR PRODUCING SLURRY, AND METHOD FOR APPLYING RELEASE AGENT

発明審査中
7閲覧数
18請求項 · 3 独立
§ Ⅰ

案件概要

発明者

Zen ITO; Masaaki HIGUCHI; Keita IMANAKA; Masamitsu KIMURA; Hiroyasu KONDO

IPC分類

C4B 41/45C4B 35/581C4B 35/584C4B 41/50C11D 11/H5K 1/3

CPC分類

C4B41/459C4B35/581C4B35/584C4B41/5064C11D11/94H5K1/306C4B2235/3865C4B2235/3873

A ceramic substrate according to an embodiment has a first surface as a front surface and a second surface as a back surface, when a midpoint of a line segment connecting a central portion Pof the first surface and a central portion Pof the second surface is defined as a midpoint portion C, an amount of a component of a release agent measured at the central portion Pof the first surface or the central portion Pof the second surface is five times or more an amount of the component of the release agent measured at the midpoint portion C. A ratio P/Pbetween the amount of the component of the release agent measured at the central portion Pand the amount of the component of the release agent measured at the central portion Ppreferably satisfies 0.5≤P/P≤2.

原文(中国語)

A ceramic substrate according to an embodiment has a first surface as a front surface and a second surface as a back surface, when a midpoint of a line segment connecting a central portion Pof the first surface and a central portion Pof the second surface is defined as a midpoint portion C, an amount of a component of a release agent measured at the central portion Pof the first surface or the central portion Pof the second surface is five times or more an amount of the component of the release agent measured at the midpoint portion C. A ratio P/Pbetween the amount of the component of the release agent measured at the central portion Pand the amount of the component of the release agent measured at the central portion Ppreferably satisfies 0.5≤P/P≤2.