MANUFACTURING METHOD OF SEMICONDUCTOR STRUCTURE

発明審査中
15請求項 · 2 独立
§ Ⅰ

案件概要

IPC分類

H1L 21/2H1L 21/308H1L 21/324H1L 21/3105

CPC分類

H1L21/228H1L21/308H1L21/324H1L21/2123H1L21/2554H1L21/31051

A manufacturing method of a semiconductor structure is provided. The method includes following steps. A substrate is provided. A trench is formed in the substrate, wherein an active area is protruded from the substrate and the active has a first width. A thin silicon layer is formed on the active area and a sidewall of the trench. A first oxide layer is formed on the thin silicon layer by providing oxygen airflow, wherein the first oxide layer is formed in a range of 400°C to 600°C. A second oxide layer is formed to fill the trench and cover the active area, wherein the second oxide layer is formed at a temperature higher than the first oxide layer. And an anneal process is performed to crystalize the thin silicon layer.

原文(中国語)

A manufacturing method of a semiconductor structure is provided. The method includes following steps. A substrate is provided. A trench is formed in the substrate, wherein an active area is protruded from the substrate and the active has a first width. A thin silicon layer is formed on the active area and a sidewall of the trench. A first oxide layer is formed on the thin silicon layer by providing oxygen airflow, wherein the first oxide layer is formed in a range of 400°C to 600°C. A second oxide layer is formed to fill the trench and cover the active area, wherein the second oxide layer is formed at a temperature higher than the first oxide layer. And an anneal process is performed to crystalize the thin silicon layer.

外部リソース