NiCu/La-ZEOLITE CATALYST

발명심사 중
1조회수
20청구항 · 3 독립항
§ Ⅰ

개요

발명자

Kyriaki POLYCHRONOPOULOU; Mariam Ahmed MOHAMMED; Sara Ishaq ALKHOORI

IPC 분류

B1J 29/78B1J 35/40B1J 35/61B1J 35/77B1J 37/2C10G 3/

CPC 분류

B1J29/7815B1J35/40B1J35/615B1J35/77B1J37/205C10G3/49B1J2235/15C10G2300/1011C10G2300/70C10G2400/4

A method of manufacturing a catalyst includes mechanochemically processing an input material to generate a processed material, where the input material comprises a support and loading the processed material with a loading material. The support is a zeolite, a Beta zeolite, or a H-Beta zeolite and the loading material comprises nickel (Ni) or nickel-copper (NiCu). Lanthanum oxide (LaO) is a promoter for the catalyst. A first interface of a NiCu/La-zeolite catalyst is generated when the loading material further includes the promoter; and a second interface of a NiCu/La-zeolite catalyst is generated when the input material further includes the promoter.

원문 (중국어)

A method of manufacturing a catalyst includes mechanochemically processing an input material to generate a processed material, where the input material comprises a support and loading the processed material with a loading material. The support is a zeolite, a Beta zeolite, or a H-Beta zeolite and the loading material comprises nickel (Ni) or nickel-copper (NiCu). Lanthanum oxide (LaO) is a promoter for the catalyst. A first interface of a NiCu/La-zeolite catalyst is generated when the loading material further includes the promoter; and a second interface of a NiCu/La-zeolite catalyst is generated when the input material further includes the promoter.