METHOD FOR REMOVING ALUMINUM AND METHOD FOR RECOVERING METALS

발명심사 중
18청구항 · 1 독립항
§ Ⅰ

개요

발명자

Naoki HIGUCHI; Kei SHIKADA

IPC 분류

C22B 21/C22B 1/2C22B 1/248C22B 3/C22B 7/C22B 23/C22B 26/12C22B 47/H1M 10/54

CPC 분류

C22B21/23C22B1/2C22B1/248C22B7/7C22B21/7C22B23/5C22B23/43C22B26/12C22B47/H1M10/54

Provided are a method for removing aluminum which can effectively remove aluminum, and a method for recovering metals. A method for removing aluminum includes a leaching step of bringing a raw material obtained from lithium ion battery waste, the raw material having battery powder containing at least aluminum and nickel and/or cobalt, into contact with an acidic leaching solution to leach the battery powder to obtain a leached solution, wherein a molar ratio of fluorine to aluminum (F/Al molar ratio) of the raw material is 1.3 or more, and wherein, in the leaching step, the acidic leaching solution contains calcium and fluorine, aluminum is precipitated with calcium and fluorine, and the resulting precipitate is contained in a leached residue.

원문 (중국어)

Provided are a method for removing aluminum which can effectively remove aluminum, and a method for recovering metals. A method for removing aluminum includes a leaching step of bringing a raw material obtained from lithium ion battery waste, the raw material having battery powder containing at least aluminum and nickel and/or cobalt, into contact with an acidic leaching solution to leach the battery powder to obtain a leached solution, wherein a molar ratio of fluorine to aluminum (F/Al molar ratio) of the raw material is 1.3 or more, and wherein, in the leaching step, the acidic leaching solution contains calcium and fluorine, aluminum is precipitated with calcium and fluorine, and the resulting precipitate is contained in a leached residue.