CNIPA.AI
검색으로 돌아가기
기록

METHOD FOR PRODUCING PROFILED FIBERS HAVING LOW BROKEN FILAMENT RATE BY POLYESTER FDY PROCESS

발명심사 중
1조회수
11청구항 · 1 독립항
§ Ⅰ

개요

발명자

Jianguang ZHANG; Yonglin ZOU; Xinzhao HU; Lixin YIN; Shunjun YANG; Chengqian ZHU; Yu LI; Shouzuo LIU

IPC 분류

D1H 13/30D1H 13/2D1H 13/4D1H 13/32

CPC 분류

D1H13/306D1H13/2D1H13/4D1H13/32

A method for preparing profiled fibers with low lousiness rate by a polyester FDY process is provided, when preparing profiled fibers by the FDY process, during the operation of a yarn path, the horizontal and longitudinal positions of wire guide ceramic pieces on the pre-entangling wire guide frame are adjusted to maintain vertical alignment of the filament bundle in the pre-entangling device and achieve optimal jitter effect, to prepare profiled fibers with a low lousiness rate; when the profiled fibers are triangular profiled fibers, the lousiness rate is 0.35-0.65%; when the profiled fibers are trilobal profiled fibers, the lousiness rate is 0.85-1.25%; when the profiled fibers are flat profiled fibers, the lousiness rate is 0.5-0.85%.

원문 (중국어)

A method for preparing profiled fibers with low lousiness rate by a polyester FDY process is provided, when preparing profiled fibers by the FDY process, during the operation of a yarn path, the horizontal and longitudinal positions of wire guide ceramic pieces on the pre-entangling wire guide frame are adjusted to maintain vertical alignment of the filament bundle in the pre-entangling device and achieve optimal jitter effect, to prepare profiled fibers with a low lousiness rate; when the profiled fibers are triangular profiled fibers, the lousiness rate is 0.35-0.65%; when the profiled fibers are trilobal profiled fibers, the lousiness rate is 0.85-1.25%; when the profiled fibers are flat profiled fibers, the lousiness rate is 0.5-0.85%.