CNIPA.AI
검색으로 돌아가기
기록

PRODUCTION OF SEMI-SOLID ELECTRODES VIA ADDITION OF ELECTROLYTE TO MIXTURE OF ACTIVE MATERIAL, CONDUCTIVE MATERIAL, AND ELECTROLYTE SOLVENT

발명심사 중
1조회수
24청구항 · 5 독립항
§ Ⅰ

개요

발명자

Junzheng CHEN; Landon OAKES; Naoki OTA; Matthew Bonju LIM

IPC 분류

H1M 10/585H1M 4/4H1M 10/568H1M 10/569

CPC 분류

H1M10/585H1M4/404H1M10/568H1M10/569H1M2300/28Y10T29/49108

Embodiments described herein relate generally to semi-solid electrodes, and methods of producing the same. In some embodiments, a method of forming a semi-solid electrode can include mixing an active material, a conductive material, and an electrolyte solvent to produce a semi-solid material. The electrolyte solvent is free of electrolyte salt. The method further includes dispensing the semi-solid material onto a current collector and wetting the semi-solid material with an electrolyte solution to form the semi-solid electrode. In some embodiments, the wetting can be via spraying. In some embodiments, the electrolyte salt can have a concentration in the electrolyte solution of at least about 1 M, at least about 2 M, or at least about 3 M. In some embodiments, the solvent can include ethyl methyl carbonate (EMC), ethylene carbonate (EC), propylene carbonate (PC), dimethyl carbonate (DMC), gamma-Butyrolactone (GBL), or any combination thereof.

원문 (중국어)

Embodiments described herein relate generally to semi-solid electrodes, and methods of producing the same. In some embodiments, a method of forming a semi-solid electrode can include mixing an active material, a conductive material, and an electrolyte solvent to produce a semi-solid material. The electrolyte solvent is free of electrolyte salt. The method further includes dispensing the semi-solid material onto a current collector and wetting the semi-solid material with an electrolyte solution to form the semi-solid electrode. In some embodiments, the wetting can be via spraying. In some embodiments, the electrolyte salt can have a concentration in the electrolyte solution of at least about 1 M, at least about 2 M, or at least about 3 M. In some embodiments, the solvent can include ethyl methyl carbonate (EMC), ethylene carbonate (EC), propylene carbonate (PC), dimethyl carbonate (DMC), gamma-Butyrolactone (GBL), or any combination thereof.