CERAMIC SUBSTRATE, CERAMIC CIRCUIT BOARD, SEMICONDUCTOR DEVICE, METHOD FOR PRODUCING SLURRY, AND METHOD FOR APPLYING RELEASE AGENT

발명심사 중
18청구항 · 3 독립항
§ Ⅰ

개요

발명자

Zen ITO; Masaaki HIGUCHI; Keita IMANAKA; Masamitsu KIMURA; Hiroyasu KONDO

IPC 분류

C4B 41/45C4B 35/581C4B 35/584C4B 41/50C11D 11/H5K 1/3

CPC 분류

C4B41/459C4B35/581C4B35/584C4B41/5064C11D11/94H5K1/306C4B2235/3865C4B2235/3873

A ceramic substrate according to an embodiment has a first surface as a front surface and a second surface as a back surface, when a midpoint of a line segment connecting a central portion Pof the first surface and a central portion Pof the second surface is defined as a midpoint portion C, an amount of a component of a release agent measured at the central portion Pof the first surface or the central portion Pof the second surface is five times or more an amount of the component of the release agent measured at the midpoint portion C. A ratio P/Pbetween the amount of the component of the release agent measured at the central portion Pand the amount of the component of the release agent measured at the central portion Ppreferably satisfies 0.5≤P/P≤2.

원문 (중국어)

A ceramic substrate according to an embodiment has a first surface as a front surface and a second surface as a back surface, when a midpoint of a line segment connecting a central portion Pof the first surface and a central portion Pof the second surface is defined as a midpoint portion C, an amount of a component of a release agent measured at the central portion Pof the first surface or the central portion Pof the second surface is five times or more an amount of the component of the release agent measured at the midpoint portion C. A ratio P/Pbetween the amount of the component of the release agent measured at the central portion Pand the amount of the component of the release agent measured at the central portion Ppreferably satisfies 0.5≤P/P≤2.