一种Au-Pd/CdS纳米棒及合成方法

InventionActive
9Claims · 1 independent
§ Ⅰ

Dossier Overview

Inventor

黄硕; 沈璟昊; 谢宇; 易龙辉; 戴玉华

IPC Classification

B01J 27/045 (2006.01)C01G 11/02 (2006.01)B82Y 40/00 (2011.01)B82Y 30/00 (2011.01)B01J 35/39 (2024.01)B01J 35/30 (2024.01)B01J 35/45 (2024.01)

本发明公开了一种Au‑Pd/CdS纳米棒及合成方法,包括步骤:S1、将Cd(NO)·4HO与硫脲按1:(2.5~3.5)摩尔比溶于乙二胺,180~200℃水热反应18~36h制备CdS纳米棒;S2、将CdS纳米棒分散于水中,加入含HAuCl·3HO和PbCl的混合溶液,调控Au/Pd摩尔比为1:9至9:1,搅拌吸附8~12h后加入NaBH室温还原10~15h,经洗涤、干燥获得Au‑Pd/CdS复合催化剂。