本发明涉及钢铁冶金技术领域,具体公开了一种300t转炉冶炼冷轧板钢种薄板坯连铸机直上工艺方法,实现300t大型转炉冶炼冷轧板系列钢种薄板坯连铸机近直上的目的;取消RH真空工序、取消LF精炼工序深精炼工艺时间,将300吨冷轧板系列钢种的在放钢后进行极简渣改质,压缩钢包盛钢周期由150min到60min;利用转炉16的低碳氧积,通过转炉终点精准控制(终点碳≤0.040%、终点氧≤420ppm、终点磷≤0.028%)和创新的出钢脱氧合金化工艺方式,实现铝收得率稳定、转炉氩站渣达到近终态水平;开发精炼渣改质工艺;建立钙处理与软吹标准化工艺参数,实现夹杂物充分变性,减少冷轧板表面翘皮缺陷,提高成材率。